Above: SEM photo. Upper half  is oxidized area. Matrix of Gamma oxidized because of  the reduction of Cr in the matrix. Below: OM photo.  Oxidized/unoxidized interface. Sigma phase is Cr/Fe compound which is more resistant to high temp oxidation than the Gamma matrix.
 
 
 
 

 

This heat resistant steel welded pipe failed in 2 months. Normal service life is 12 months.

 