- Dec 02 Wed 2009 09:08
郭先生 流道切片
- Nov 24 Tue 2009 21:46
FCD 淬火硬度不足
- Nov 13 Fri 2009 22:22
鑄鐵的 CCT for grey iron
Photos taken from pig iron that froze in iron mold. Light color areas are upper temp transformation product, fine pearlite; while dark color areas are lower temp transformation products, Martensite and Retained Austenite.
- Nov 07 Sat 2009 22:40
逆白口 inverse chill
- Oct 23 Fri 2009 09:55
假調質 Fake Q/T steel
高溫軋延後直接空冷, 鋼材硬度會有HRC 20~30. 有黑心廠商把此冒充為調質鋼賣, 大賺黑心錢. 這種鋼材內部的碳化物形貌(有尖銳者,有薄片形者), 對韌性極具殺傷力, 直接使用還不會出問題, 淬火後使用一定會出問題, 因為這些碳化物會引發微裂, 導致破裂. 高週波淬火也很難不裂, 常使熱處理者背黑鍋. 即使淬後未裂, 日後還是會裂. 買鋼材時要事先約定好, 千萬不要被矇騙.
- Oct 23 Fri 2009 00:03
素材 晶界碳化物 作祟H13
- Oct 22 Thu 2009 23:39
素材 晶界碳化物 的遺害